Institute of Physics of Materials AS CR, v. v. i. > Projects > The link between microstructure and creep behaviour of precipitate strengthened alloys processed by ECAP

The link between microstructure and creep behaviour of precipitate strengthened alloys processed by ECAP

InvestigatorRNDr. Milan Svoboda, CSc.
Number of ProjectP108/11/2260
AgencyGrantová agentura České republiky
Duration2010-12-31 - 2014-12-30

Anotace
At present, the equal-channel angular pressing (ECAP) is the most developed of all potential severe plastic deformation (SPD) techniques for achieving very significant grain refinement in metallic materials. Despite enormous research effort in ECAPed materials so far only very limited investigations on the link between their microstructure and creep behaviour have been carried out. Thus, this project is initiated to provide detailed examination of the effect of precipitates on the microstructural stability and creep resistance of the selected precipitate strengthened aluminium and copper based alloys processed by SPD, mostly ECAP. The results should develop optimum processing schemes for attaining the desired creep properties of SPD processed materials.


2015

Buršík J., Buršíková V., Svoboda M.: Local Mechanical Properties of Cu-Co Alloys with Coherent Co Precipitates. Key Eng. Mater. 662 (2015) 15-18



2014

Kvapilová M., Dvořák J., Král P., Svoboda M., Sklenička V.: Application of the Monkman-Grant Relationship for Ultrafine-Grained Metallic Materials. Key Eng. Mater. 577-578 (2014) 137-140

Buršík J., Král P., Svoboda M., Dvořák J., Sklenička V.: Nanoindentation and microstructural study of Cu-Co alloys after severe plastic deformation. Key Eng. Mater. 592-593 (2014) 720-723

Blum W., Dvořák J., Král P., Eisenlohr P., Sklenička V.: Effect of grain refinement by ECAP on creep of pure Cu. Mater. Sci. Eng. A 590 (2014) 423-432

Sklenička V., Král P., Dvořák J., Kvapilová M., Svoboda M.: Microstructure evolution and creep behavior in ECAP processed metallic materials. Mater. Sci. Forum 783-786 (2014) 2689-2694

Buršík J., Buršíková V., Svoboda M., Král P., Dvořák J., Sklenička V.: Microstructure and local mechanical properties of Cu-Co alloys after severe plastic deformation. Key Eng. Mater. 586 (2014) 100-103

Blum W., Dvořák J., Král P., Eisenlohr P., Sklenička V.: What is stationary deformation of pure Cu?. J. Mater. Sci. 49 (2014) 2987-2997



2013

Dvořák J., Sklenička V., Betekhtin V., Kadomtsev A., Král P., Kvapilová M., Svoboda M.: The effect of high hydrostatic pressure on creep behaviour of pure Al and a Cu-0.2 wt% Zr alloy processed by ECAP. Mater. Sci. Eng. A 584 (2013) 103-113

Sklenička V., Kuchařová K., Kvapilová M., Svoboda M., Král P., Vidrich G.: Creep in an electrodeposited nickel. J. Mater. Sci. 48 (2013) 4780-4788