Creep test system Zwick/Roell - Messphysik KAPPA LA spring 50kN, with furnace MAYTEC up to 1200 C
Contact person: Ing. Petr Dymek, Ph.D.
Creep test system Zwick/Roell - Messphysik KAPPA LA spring 50kN, with furnace MAYTEC up to 1200 C, testing in air and Ar protective atmosphere

  • tensile creep testing

  • compressive creep testing

  • stress relaxation testing

  • strain measurement with MAYTEC extensometer with 11-50 mm gauge length, with 10 mm measurement range and 0.1 m resolution

  • testing of specimens with threaded heads M4, M5, M6, M9, M10, M12

  • testing of flat specimens with slot 6mm

  • testing of compressive specimens, from ⌀3mm, L= 4mm to ⌀10mm, L=20mm in reversal cage